Stainless steel — EN 1993-1-4
Stainless member resistance and deflection to EN 1993-1-4 — how a material is read as stainless, what is checked, and what is left to you.
Design checks 8 min read
Two modules verify stainless steel members to EN 1993-1-4:2006 with A1:2015 and
A2:2020: en1993-1-4.member-resistance at ULS and en1993-1-4.deflection at SLS. They
are not a variation of the EN 1993-1-1 check. The partial factors,
class limits, reduction factors, buckling curves, lateral-torsional buckling, interaction and
shear all differ. Cross-sections stay §6.2 of EN 1993-1-1, which EN 1993-1-4 §5.1(1) keeps,
with this part's rules fed in.
Austenitic, duplex and ferritic steels are covered. EN 1993-1-4:2025 replaces the 2006 text and is not implemented yet; each result states the rule set it used.
Both modules are in New check under EN 1993-1-4, in every plan. Each counts towards the plan's design checks per project.
How a material reads as stainless
A material has no grade field, so the check reads its words, in this order:
- The stated standard. EN 10088 reads stainless. EN 10025, EN 10210, EN 10219, EN 10080 and ASTM A36, A572 and A992 read carbon steel, whatever the name says.
- The name and description. A designation that can only be stainless wins: 1.4301, S30400, X5CrNi18-10, 316L, ČSN 17 240. Then a clear carbon grade: "S355 korozivzdorná" is S355. Then words such as stainless, nerez or korozivzdorná, and a bare 304 or 2205 where the whole field is that number.
The library's stainless materials state their standard, so they need nothing more. If you add your own, name the grade. Every result names what the material was read as, so a miss is visible. A material called only "Plate" stays carbon steel.
The checks refuse each other's materials. EN 1993-1-4 refuses a material not read as stainless, and EN 1993-1-1 and AISC 360 refuse one that is.
| What the material gives | What the check does |
|---|---|
| A grade in A1 Tables 2.1 and 2.2 | Its family, and as they stand |
| A grade outside those tables | Its family, with raised by 10 % by A1 2.1.1(1), and a message |
| Words that say stainless with no grade or family | Not verified until you name the grade, or set Family on the check. A family is never guessed: A2 Table 5.3 differs by it, in both directions |
| other than EN 1993-1-4 2.1.3 gives (200 000 MPa, 220 000 ferritic, 195 000 for some austenitic grades) | The material's value is used, with a message |
is read as you entered it. A1 Table 2.1 replaces Table 3.1's thickness reduction with columns by product form, each with its own thickness limit, so the library carries one material per grade and product form, and the CP350 and CP500 cold-worked values of Table 2.2. If the section is thicker than that column allows, or is above every column of the grade, the result says so.
Member resistance
| Check | Clause | What the module does |
|---|---|---|
| Cross-section | EN 1993-1-1 §6.2, kept by §5.1(1) | Tension, compression, bending, shear, torsion and their interactions, at , on this part's classes and on P413 Table 5.5's shear areas with |
| Flexural buckling | §5.4, A2 Table 5.3 | and by the section, its fabrication and the family |
| Torsional and torsional-flexural buckling | §5.4 | At the minor-axis and of Table 5.3 |
| Lateral-torsional buckling | §5.4.3 | , , 0.34 for cold formed or hollow sections and 0.76 otherwise. No of EN 1993-1-1 §6.3.2.3: the note to §5.4.1 says it doesn't apply |
| Bending and compression | §5.5, (5.13) to (5.17) | and with their floor of 1.2. No , and no Annex A or B |
| Biaxial bending, no compression | SCI P413 §6.5.2 | (5.16) and (5.17) at the floor. A hollow section reads P413 (6.63) at , a tube on the resultant moment |
| Tension and bending | SCI P413 (6.55) | At the most stressed section |
| Shear buckling | §5.6 after A1 | with η, 1.20 by default, the end post as on the EN 1993-1-1 check, and on request the stiffener spacing a per member, with the flange contribution of an I |
Where a clause number after A1 or A2 isn't known to us, or EN doesn't say how something is read, the result names the source used, usually SCI P413, the Design Manual for Structural Stainless Steel. The reduction factor and §5.6's rules are read through P413, which states them as A1's. P413 values that go past EN stay options: k, hollow on the check picks EN 1993-1-4 (the default) or SCI P413 D₁–D₃ (not EN), a lower set for RHS and CHS.
Classification
Table 5.2 of EN 1993-1-4 has its own numbers, and its carries :
| Part | Class 1 | Class 2 | Class 3 |
|---|---|---|---|
| Internal, compression | |||
| Internal, bending | |||
| Outstand, compression | |||
| Tube, compression | |||
| Tube, bending, mm |
Hollow section walls take . A cold formed channel's outstand is its whole leg, . Under N + M, comes from N alone by P413 p. 57, and the result says so. Elements past 50 with an edge free or 400 with both held are outside the rules, and the member reads not verified. Past about 30 and 75 they carry a note about visible distortion.
Class 4 I and H sections, hollow sections and a channel under are verified on their effective section by §5.2.3. A section can state its own class in the section editor. Stated buckling curves are EN 1993-1-1's letters and are not used here.
Buckling curves
| Section | , |
|---|---|
| Hot rolled or welded open section, welded box | Major axis 0.49, 0.2; minor axis 0.76, 0.2 |
| Cold formed angle or channel | 0.76, 0.2 |
| Cold formed RHS | 0.49, 0.3; ferritic 0.49, 0.2 |
| Hot finished RHS | 0.49, 0.2; ferritic 0.34, 0.2 |
| Cold formed CHS | 0.49, 0.2 |
| Hot finished CHS | 0.49, 0.2; ferritic 0.34, 0.2 |
| Welded CHS | 0.49, 0.2, assumed: A2 has no row for one |
Any other cold formed section has no row, and reads not verified in compression.
Fabrication on the check matters here. A catalogue's hollow sections state hot finished, but stainless tubes are usually cold formed, so a tube whose make isn't stated takes the lower of the family's two rows until Fabrication says otherwise, with a message.
M_cr, load height and buckling lengths
These work as on the EN 1993-1-1 check, with P413's Tables E.1 and E.2 in place of NB.3: M_cr from offers P413 table, else eigenvalue, Eigenvalue always and C_1 = 1.0. The load's position applies the same way: top flange until the member says otherwise, from the row, on a hollow section. Buckling lengths come from the same three sources.
Partial factors and the annex
| Factor | EN 1993-1-4 Table 5.1 | Applies to |
|---|---|---|
| 1.10 | Cross-section resistance | |
| 1.10 | Member buckling and shear buckling |
These are distinct from the EN 1993-1-1 values, where the recommended ones are 1.00: a project on γ_M0 = 1.00 still reads 1.10 here unless you change it. We hold an annex's stainless factors for Bulgaria, the Czech Republic, Finland, Italy, Poland, Spain and the UK, all of which adopt Table 5.1. For any other annex the setup says the value isn't held and EN's own stands. See National annexes.
Deflection
en1993-1-4.deflection checks a member against the same limit rows as the
EN 1990 deflection check, but takes the
non-linear stress-strain curve into account through the secant modulus of EN 1993-1-4 §4.2.
At the worst station it takes the stress in the tension and compression flanges from , then:
The solver's linear deflection is scaled by , using that lowest modulus over the whole member as §4.2(9) allows. comes from Table 4.1, longitudinal. A grade not in the table takes P413 Table 6.4's family value: 7 austenitic, 8 duplex, 14 ferritic, marked as assumed. A Class 4 section reads and in its stresses and scales by as well.
Deflection reads displacements, so this check needs an analysis and can't run on forces entered by hand.
Not covered
Each of these is raised as a message on the check or is a stated assumption of the module:
- Web crippling at supports and under point loads (P413 §6.4.4). It needs the bearing length and load type, which the model does not record.
- Shear lag and flange curling. Each is stated on a member it reaches, with the numbers, and left for you to check.
- Stiffened plates and distortional buckling to EN 1993-1-3.
- Angles in compression through one leg. Annex BB.1.2's hasn't been verified for stainless, so they read not verified. So does an eccentricity modelled as an element offset. Angle connection set to Concentric: the force passes the centroid is verified.
- Class 4 circular hollow sections in compression or bending, and any tube over mm in bending past : EN 1993-1-4 points to EN 1993-1-6. A Class 4 tube in shear or torsion reads EN 1993-1-6 §8.5.
- Class 4 channels in compression, and Class 4 angles and tees outside pure tension.
- Member stability with a bimoment. With warping torsion in the analysis, the section reads the bimoment and both torques by EN 1993-1-1 §6.2.7, as the carbon steel check does. Neither SCI P413 nor EN 1993-1-4 has a member rule with torsion, so the member's buckling with it isn't verified, and the check says so.
- Net section fracture, connections, fire and fatigue.
Related
Steel — EN 1993-1-1 for the shared M_cr and load-height rules; Serviceability checks for limit rows and how they are read; Sections and materials for the material library.
Something wrong or unclear on this page? Tell us, and it gets corrected.